Electrolyzer for Brine Electrochlorinators

➤ Batch type 8 hours per day
Capacity Single electrolyzer, having the production capacity of available Cl2 per hour is
1. Minimum size: 6.25 grams
2. Maximum size: 125 grams
Concentration 6000 ppm to 8000 ppm of Cl2
Design PPE, CTE, PP & ME
Polarity Normal & Reverse
Substrate 1. Titanium sheet / plate as per ASTM B 265 Gr.1
2. Titanium tube / pipe as per ASTM B 338/337 Gr.1
3. Titanium expanded mesh as per ASTM B 265 Gr.1
4. Titanium rods as per ASTM B 348 Gr.1
Catalyst Platinum group precious metal mixed oxides
Application Disinfection
Replacement Denora, Mac, Siemens, Sal-Chlor & Many more.
➤ Batch type 20 hours per day
Capacity Single electrolyzer, having the production capacity of available Cl2 per hour is
1. Minimum size: 25 grams
2. Maximum size: 1000 grams
Concentration 7000 ppm to 8000 ppm of Cl2
Design PPE
Polarity Normal & Reverse
Substrate 1. Titanium sheet / plate as per ASTM B 265 Gr.1
2. Titanium rods as per ASTM B 348 Gr.1
Catalyst Platinum group precious metal mixed oxides
Application Disinfection
➤ Batch type 24 hours per day
Capacity Single electrolyzer, having the production capacity of available Cl2 per hour is
1. Minimum size: 50 grams
2. Maximum size: 100 grams
Concentration 6000 ppm to 8000 ppm of Cl2
Design CTE
Polarity Normal
Substrate 1. Titanium sheet / plate as per ASTM B 265 Gr.1
2. Titanium rods as per ASTM B 348 Gr.1
Catalyst Platinum group precious metal mixed oxides
Application Disinfection
Product 1 Product 1 Product 1 Product 1 Product 1 Product 1